2 Comments


  1. Hi! my name is D.K Shin & I’m engineer who works in nuclear industry(south korea)
    first of all it is useful information to me & I have some question!
    we have two vacuum furnace of graphit heat element in ipsen (metal master) we perform brazing by using nickel paste in nuclear field, as you know quaility is most important factor in nuclear industry
    but in theseday we have problem about attached picture, we found surface of product, it seems like black spot & only found using blower, so if ipsen engineer experienced this similar problem, I wanna get some comment & discuss this situation
    please reply to my email (sindk85@gmail.com)
    test base metal is aisi304 & inconel718!

    Reply

    1. Hello D.K. Shin,

      Thank you for reaching out to us. We have passed on your question and information to the appropriate Ipsen expert, and he should be in contact with you shortly to discuss this issue. If you need further assistance with a technical issue, you can also email TechnicalSupport@IpsenUSA.com or call our Aftermarket Support Helpline: 1-844-Go-Ipsen (International: +1-815-332-2530).